Galvanizasyon cho-plonje se yon pwosesis kouch asye ak yon kouch zenk mens, ki sèvi kòm yon baryè ant asye a ak anviwònman an.

Dekri teren

Kalite Materyèl-No. Kouch posib Direksyon tès la Pwen sede Rp0,2 (MPa)
 
Fòs rupture Rm (MPA) Elongasyon A80 (an %) r-Valè
min.
n-Valè
min
DX51D 1.0917 +Z, +ZF, +ZA, %+AZ+AS+AS, +ZM Q - 270-500 22 - -
DX52D 1.0918 +Z, +ZF, +ZA, +AZ, +AS, +ZM Q 140-300 270-420 26 - -
DX53D 1.0951 +Z, +ZF, +ZA, %+AZ+AS+AS, +ZM Q 140-260 270-380 30 - -
DX54D 1.0952 +Z, +ZA Q 120-220 260-350 36 1,6 0,18
DX54D 1.0952 +ZF, +ZM Q 120-220 260-350 34 1,4 0,18
DX54D 1.0952 +AZ Q 120-220 260-350 36 - -
DX54D 1.0952 +AS Q 120-220 260-350 34 1,4 0,18
Kalite Materyèl-No. Kouch posib Direksyon tès la Pwen sede Rp0,2 (MPa)
 
Fòs rupture Rm (MPA) Elongasyon A80 (an %) r-Valè
min.
n-Valè
min
DX55D 1.0962 +AS Q 140-240 270-370 30 - -
DX56d 1.0963 +Z, +ZA Q 120-180 260-350 39 1,9 0,21
DX56D 1.0963 +ZF, +ZM Q 120-180 260-350 37 1,7 0,20
DX56d 1.0963 +AS, +AZ Q 120-180 260-350 39 1,7 0,20
DX57D 1.0853 +Z, +ZA Q 120-170 260-350 41 2,1 0,22
DX57D 1.0853 +ZF, +ZM Q 120-170 260-350 39 1,9 0,21
DX57D 1.0853 +AS Q 120-170 260-350 41 1,9 0,21
Kalite Materyèl-No. Kouch posib Direksyon tès la Pwen sede Rp0,2 (MPa)
 
Fòs rupture Rm (MPA) Elongasyon A80 (an %)
S220GD 1.0241 +Z, +ZF, +ZA, +AZ, +ZM L min. 220 min. 300 20
S250gd 1.0242 +Z, +ZF, +ZA, %+AZ+AS+AS, +ZM L min. 250 min. 330 19
S280GD 1.0244 +Z, +ZF, +ZA, %+AZ+AS+AS, +ZM L min. 280 min. 360 18
S320GD 1.0250 +Z, +ZF, +ZA, %+AZ+AS+AS, +ZM L min. 320 min. 390 17
S350gd 1.0529 +Z, +ZF, +ZA, %+AZ+AS+AS, +ZM L min. 350 min. 420 16
S390gd 1.0238 +Z, +ZF, +ZA, +AZ, +ZM L min. 390 min. 460 16
S420gd 1.0239 +Z, +ZF, +ZA, +AZ, +ZM L min. 420 min. 480 15
S450gd 1.0233 +Z, +ZF, +ZA, +AZ, +ZM L min. 450 min. 510 14
S550gd 1.0531 +Z, +ZF, +ZA, +AZ, +ZM L min. 550 min. 560 -

Regular Spangles of GI CoilGalvanized Steel Coil

Spangles regilye galvanize bobin galvanize bobin asye

 

 

Hot-plonje asye galvanised dapre DIN EN 10346

Z

Dosye pwodwi nou an gen ladan asye galvanised cho-plonje, anba ki klas DX51D a DX57D ak asye estriktirèl S220GD a S550GD yo entegre. Klas sa yo se asye mou ki nan fèy galvanised cho-plonje epi yo karakterize pa fòmabilite ekselan yo. Yo ka itilize pou desen gwo twou san fon ak koube. Pwopriyete mekanik yo nan klas asye endividyèl yo karakterize pa nivo nan fòs sede ak fòs rupture kòm byen ke pa garanti valè minimòm de elongasyon nan kraze.

Asye mou yo ka klase jan sa a.

DX51D: Machin pliye bon jan kalite

DX52D: bon jan kalite desen

DX53D: bon jan kalite desen gwo twou san fon

DX54D: espesyal bon jan kalite desen gwo twou san fon

DX55D: Espesyal bon jan kalite desen gwo twou san fon (sèlman + AS)

DX56D: Espesyal bon jan kalite desen gwo twou san fon

DX57D: Ekstrèm bon jan kalite desen gwo twou san fon

Pou cho-tranpe kouvwi teren ak fèy, mak inifòm Ewopeyen sa yo yo te prezante.

Z zenk kouch (99% Zn)

ZF kouch alyaj zenk-fè (Galvannealed)

ZA kouch zenk-aliminyòm (Zn + 5% Al)

AZ aliminyòm-zenk kouch (55% Al + 1.6% Si + Zn)

AS aliminyòm-silikon kouch (11% Si + Al)

ZM zenk-mayezyòm kouch (1-2% Mg + 1-2% Al + Zn)

Kondisyon kouch
Tablo ki anba yo montre kondisyon kouch posib yo.

Zenk kouch konpoze (+ Z)

Faktè kouvri karakteristik Valè tipik nan µm Pòte Dansite
nan g/cm³
Z100 7 5-12 7,1
Z140 10 7-15 7,1
Z200 14 10-20 7,1
Z225 16 11-22 7,1
Z275 20 13-27 7,1
Z350 25 17-33 7,1
Z450 32 22-42 7,1
Z600 42 29-55 7,1

Mas nan alyaj zenk-fè (+ ZF)

Faktè kouvri karakteristik Valè tipik nan µm Pòte Dansite
nan g/cm³
ZF100 7 5-12 7,1
ZF120 8 6-13 7,1

Mas nan alyaj zenk-aliminyòm (+ ZA)

Faktè kouvri karakteristik Valè tipik nan µm Pòte Dansite
nan g/cm³
ZA095 7 5-12 6,6
ZA130 10 7-15 6,6
ZA185 14 10-20 6,6
ZA200 15 11-21 6,6
ZA225 20 15-27 6,6
ZA300 23 17-31 6,6

Mas de Zenk-Mayesium-Alloy (+ ZM) 1/2

Faktè kouvri karakteristik Valè tipik nan µm Pòte Dansite
nan g/cm³
ZM060 4,5 4-8 6,2-6,6
ZM070 5,5 4-8 6,2-6,6
ZM080 6 4-10 6,2-6,6
ZM090 7 5-10 6,2-6,6
ZM100 8 5-11 6,2-6,6
ZM120 9 6-14 6,2-6,6
ZM130 10 7-15 6,2-6,6
ZM140 11 8-16 6,2-6,6
ZM150 11,5 8-17 6,2-6,6

Mas nan alyaj zenk-mayezyòm (+ ZM) 2/2

Faktè kouvri karakteristik Valè tipik nan µm Pòte Dansite
nan g/cm³
ZM160 12 8-17 6,2-6,6
ZM175 13 9-18 6,2-6,6
ZM190 15 10-20 6,2-6,6
ZM200 15 10-20 6,2-6,6
ZM250 19 13-25 6,2-6,6
ZM300 23 17-30 6,2-6,6
ZM310 24 18-31 6,2-6,6
ZM350 27 19-33 6,2-6,6
ZM430 35 26-46 6,2-6,6

Mas aliminyòm-zenk-alyaj (+ AZ)

Faktè kouvri karakteristik Valè tipik nan µm Pòte Dansite
nan g/cm³
Az100 13 9-19 3,8
Az150 20 15-27 3,8
Az185 25 19-33 3,8

Mas nan alyaj aliminyòm-Silisyòm (+ AS)

Faktè kouvri karakteristik Valè tipik nan µm Pòte Dansite
nan g/cm³
AS060 10 7-15 3,0
AS080 14 10-20 3,0
AS100 17 12-23 3,0
AS120 20 15-27 3,0
AS150 25 19-33 3,0

 

Pake estanda navigab la gen ladan papye kraft ki enpèmeyab ak fim plastik andedan ak fèy GI deyò. Lè sa a, li mare ak bann asye. Anba a gen kèk foto pou referans ou.