+8615824687445
Kay / Konesans / Detay yo

May 12, 2025

Ki sa ki BS EN 10025 S355 ak S275?

1. Klasifikasyon estanda

BS EN 10025 se adopsyon Britanik la nan estanda Ewopeyen an pou cho-woule asye estriktirèl, ki kouvri sis pati:

Pati 2: Jeneral asye estriktirèl (S275/S355)

Pati 3: Normalized/normalized-woule asye grenn jaden amann

Pati 4: Thermomekanik woule weldable asye grenn jaden

Pati 5: Dezagregasyon asye

Pati 6: Mache & apeze asye wo-sede

Konpozisyon chimik (tipik %)

Eleman S275jr S355jr Limit
C (max) 0.21 0.22 EN 10025-2
Si (max) 0.40 0.55  
MN (max) 1.50 1.60  
P (max) 0.035 0.035  
S (max) 0.035 0.035  
CEV (max) 0.40 0.45 Fòmil PCM

Diferans kle ant S275 & S355

Paramèt S275 S355
Sede fòs 275 MPa 355 MPa (↑ 29%)
Fòs rupture 410-560 MPa 470-630 MPa
Ekonomi pwa - Jiska 20% pi lejè pou menm chaj
Weldability (CEV) Pi bon (0.40 max) Bon (0.45 max)
Koute Bese Pi wo (~ 15-20% prim)