LR AH69 Batobuilding Steel Plate
| C max | Si max | Mn | P max | S max | N max. |
| 0.21 | 0.55 | 1.70 | 0.030 | 0.030 | 0.020 |
| Fòs Sede (MPa) min. | Fòs rupture (MPa) | Pwolonjman min. % | |||
| 690 | 770-940 | 14 | |||
LR DH69 Fèy asye konstriksyon bato
| C max | Si max | Mn | P max | S max | N max. |
| 0.20 | 0.55 | 1.70 | 0.025 | 0.025 | 0.020 |
| Fòs Sede (MPa) min. | Fòs rupture (MPa) | Pwolonjman min. % | |||
| 690 | 770-940 | 14 | |||
LR EH69 Bobin asye konstriksyon bato
| C max | Si max | Mn | P max | S max | N max. |
| 0.20 | 0.55 | 1.70 | 0.025 | 0.025 | 0.020 |
| Fòs Sede (MPa) min. | Fòs rupture (MPa) | Pwolonjman min. % | |||
| 690 | 770-940 | 14 | |||
LR FH69 Bobin asye konstriksyon bato
| C max | Si max | Mn | P max | S max | N max. |
| 0.18 | 0.55 | 1.60 | 0.020 | 0.020 | 0.020 |
| Fòs Sede (MPa) min. | Fòs rupture (MPa) | Pwolonjman min. % | |||
| 690 | 770-940 | 14 | |||