LR AH55 Bobin asye konstriksyon bato
| C max | Si max | Mn | P max | S max | N max. |
| 0.21 | 0.55 | 1.70 | 0.030 | 0.030 | 0.020 |
| Fòs Sede (MPa) min. | Fòs rupture (MPa) | Pwolonjman min. % | |||
| 550 | 670-830 | 16 | |||
LR DH55 Batobuilding Steel Plate
| C max | Si max | Mn | P max | S max | N max. |
| 0.20 | 0.55 | 1.70 | 0.025 | 0.025 | 0.020 |
| Fòs Sede (MPa) min. | Fòs rupture (MPa) | Pwolonjman min. % | |||
| 550 | 670-830 | 16 | |||
LR EH55 bato klas asye bobin
| C max | Si max | Mn | P max | S max | N max. |
| 0.20 | 0.55 | 1.70 | 0.025 | 0.025 | 0.020 |
| Fòs Sede (MPa) min. | Fòs rupture (MPa) | Pwolonjman min. % | |||
| 550 | 670-830 | 16 | |||
LR FH55 Marin asye plak
| C max | Si max | Mn | P max | S max | N max. |
| 0.18 | 0.55 | 1.60 | 0.020 | 0.020 | 0.020 |
| Fòs Sede (MPa) min. | Fòs rupture (MPa) | Pwolonjman min. % | |||
| 550 | 670-830 | 16 | |||